Somehow my last post didn't show up.
Anyway, it was about ddx. I tested TXP and HP5+ with DDX, but I used it 1:4 since that's what the standard dilution was on the bottle. Whoops! I got SBRs of 3 to 5.5. Useful information, but what about more normal situations? I looked under Options in the Plotter and found reciprocity failure numbers for HP5+ in DDx 1:5 and 1:6, and for TXT 1:8. What dilutions do y'all use for those film?
--shannon |
|
|
|
|
|